VitriReinforce Core-Flood Test Database
Strength gained, permeability kept — test after test. Every VitriReinforce core flood, plotted by post-treatment tensile-strength gain against regained permeability, with lithology, fluid, core length, injection conditions and measured Brazilian tensile strength. Part of a 200+ test program spanning core-flood, triaxial and conductivity testing.
Core tensile-strength gain vs. regained permeability
One point per core flood. The target is stronger rock that still flows: regained permeability of at least 100% (measured to 2% KCl) with a tensile-strength change of at least 0% against the untreated baseline (Brazilian method).
Explore the conductivity data yourself
Acid-fractured Indiana limestone, 1,000 to 10,000 psi closure stress — untreated against VitriReinforce.
Published in the SPE literature
The science behind VitriReinforce is peer-reviewed and public. Each paper opens its abstract on OnePetro. Access to full PDFs may require an SPE / OnePetro subscription.